Me Yasa Walda Mai Tsami Ke Fasawa? Danshi, Lalacewar Mold, da Dalilai Biyar Da Yasa Yawancin Masu Kaya Ba Za Su Ambaci Ba

Jagorar shugaban sashen zuwagazawar walda na exothermic— abubuwan da ke haifar da tsari guda biyar, hanyar tantancewa, da kuma hanyar gano gazawar walda mai hulɗa da za ku iya aiwatarwa kafin ku yanke komai.

TL;DR - Amsar filin a gaba
  • Yawancin lalacewar walda ta waje ba ta faruwa kwatsam ba kwata-kwata: kusan kashi 80% suna komawa ga ɗaya daga cikin dalilai guda biyar da masu samar da kayayyaki ba sa rubutawa - danshi da ya makale, lalacewar graphite, ƙarancin foda, gurɓataccen shiri na conductor, ko lokacin kunna mold mai sanyi.
  • Haɗin da ya yi kama da daidai har yanzu zai iya auna micro-ohm 800 akan micro-ohm 30-50 mai lafiya, saboda duba gani baya ganin porosity na gefen jagora ko lamination na oxide.
  • Ba za a iya sake zuba gaɓoɓin da suka lalace a wurinsu ba — a yanke aƙalla mm 50 na na'urar jagoranci ta wuce yankin da zafi ya shafa, a gano tushen abin da ya jawo hakan, sannan a sake shirya shi da wani abu a cikin tagar zagayowar aikinta ta 50-100.
  • KowaceTunanin Cadweld na nVent ERICO, tsarin yana samar da haɗin kwayoyin halitta, ba na injiniya ba - don haka duk wani yanayin gazawa wanda ke ƙirƙirar hanyar sadarwa (fim ɗin danshi, lamination na oxide, void) yana kayar da fasahar daga ciki.
  • Namulayin walda mai zafian ƙididdige shi don zagayowar 50-100 tare da haɗin gwiwa 80-100 da ake amfani da su a filin, an ƙera shi da graphite mai inganci don haka ramin yana da haƙuri na dogon lokaci - amma mold a wajen wannan taga ba mold bane, alhaki ne.
  • Gudanar da hulɗar hulɗaGanewar Lalacewar Waldaa ƙasa kafin ka yanke haɗin gwiwa ɗaya - zaɓi alamar da ka gani a wurin kuma ka gano mafi kusantar dalilin da kuma matakan magancewa nan take.

Makonni uku da suka gabata, wani ɗan kwangila a Cebu ya aiko min da hotuna da ƙarfe 11 na dare agogon yankin. An zuba haɗin exothermic guda ɗari biyu a kwata na baya a kan grid ɗin ƙasa na tashar ƙasa mai ƙarfin 33 kV. An fara aikin washegari da safe. Rabin haɗin sun yi kyau. Sauran rabin suna da ƙananan furanni a gefen hanyar fita daga jagorar kuma suna auna tsakanin micro-ohm 600 zuwa 900, idan aka kwatanta da 30 zuwa 50 mai lafiya a rabin da ya dace. Mai samar da su - ba mu ba - ya isar da su - ba mu ba - ba.foda na ƙarfe na waldaa kan wani jirgin ruwa da ke kan tashar jiragen ruwa ta Manila tsawon kwanaki uku na ruwan sama. Babu wanda ya buɗe ko da kwantenar guda ɗaya don dubawa.

Wannan kiran shine dalilin wannan labarin. Bayan shekaru 17 na aikin injiniyamold ɗin walda na wajega masu siye daga ƙasashen waje — da kuma shekaru 12 na kallon rahotannin aikinsu — na daina yarda da gazawar kwatsam. Abin da ya yi kama da kwatsam kusan koyaushe kuskuren tsari ne wanda babu wanda ya yi alama da shi saboda takardar ƙayyadaddun bayanai ba ta gaya musu su duba ba. Ga abin da nake aika wa duk wani ɗan kwangila wanda ya kira ni da gazawar "ɓoyayye", kamar yadda nake yi musu jagora a wurin.

Dalilin da yasa Weld ɗin Thermit da ya gaza Kusan Ba ​​Ya taɓa Faɗuwa Kamar Yadda Kuke Tunani

Dole ne in fara ƙalubalantar tsarin ginin, domin yana tsara kowace shawara da ma'aikata za su yanke game da gyara matsala. Idan wani ɗan kwangila ya kira ni da "walda da ta gaza", ina yin tambaya ɗaya kafin in yi wani abu:Shin haɗin gwiwar ya taɓa cin jarabawar juriya, ko kuma ya gaza wajen aiwatar da shi a karon farko da aka taɓa auna shi?Amsar tana canza komai, domin haɗin gwiwa da ya lalace a lokacin aiki da kuma haɗin gwiwa da ya lalace sakamakon zubar da jini matsaloli ne guda biyu daban-daban tare da tushen dalilai guda biyu daban-daban.

Bisa ga wallafe-wallafen kula da tsufa kan hanyoyin haɗin lantarki da aka binne da aka ambata a Amurka (NUREG-1800, rahoton Darussan Tsufa na Generic da aka koya don tabbatar da tsawon shekarun da aka yi na tsawon rayuwar shuke-shuke), hanyoyin lalata da aka rubuta don kowace haɗin gwiwa da aka binne sune zagayowar zafi, dumama ohmic, girgiza, da tsatsa - kuma rahoton ya bayyana a sarari cewa waɗannan hanyoyin ne da ke aiki akan hanyoyin sadarwa.Weld ɗin exothermic ba shi da alaƙa da tsufa, saboda masu jagoranci da jan ƙarfe mai narkewa suna zama ƙarfe ɗaya mai ci gaba yayin amsawar. Don haka idan haɗin exothermic da aka zubar yadda ya kamata ya gaza aiki, gazawar kusan ba ta taɓa kasancewa a cikin ƙarfen walda kanta ba - tana cikin wani ɓangare na mai gudanarwa walda da ba ta taɓa kaiwa ba, ko kuma a cikin ƙaramin rami mai amfani da zafi wanda walda da aka bari a baya saboda cajin foda ba daidai ba ne a ranar zuba.

Amsa Nugget:Lalacewar walda ta waje ko dai lahani ne daga ranar zuba (kuskuren tsari ko mai samar da kayayyaki) ko kuma sakamakon lahani daga ranar zuba (lalata da gano hanyar da aka bari ta hanyar da ba ta da kyau). Saboda fasahar tana samar da haɗin kwayoyin halitta maimakon na injiniya, gazawar haɗin gwiwa da aka zuba daidai ba kasafai ake samunta ba - wanda ke nufin kowace gazawar "ɓoye" ta cancanci a duba bayanan zubar da ruwa kafin kowa ya fara zargin sinadaran ƙasa.

Yaya "lalacewar rana" take a zahiri a cikin binciken shari'a

Haɗaɗɗun Cebu guda ɗari biyu sun koya mini tsari ɗaya da ya tsaya cak a kan kowace gazawar haɗin gwiwa da yawa da na yi tun daga lokacin. Lokacin da muka yanke haɗin gwiwa da ya gaza buɗewa muka goge ɓangaren giciye, mun ga ɗaya daga cikin ƙananan gine-gine guda biyar da ke maimaitawa, kuma kowannensu yana nuna ɗaya daga cikin dalilai biyar na tsari a cikin sauran wannan labarin:

Da zarar ka koyi karanta waɗannan ƙananan tsare-tsare guda biyar, tattaunawar warware matsaloli za ta daina zama zato. Sauran wannan jagorar za ta bi kowace matsala bisa ga tsarin da zan bincika a wurin, tare da matakin tabbatarwa wanda ke tabbatar da hakan kafin ka yanke haɗin gwiwa ɗaya.

Shin Danshi Ne Ainihin Laifi Idan Walda Mai Ruwa Ya Fasa?

Danshi shine gazawar da nake fuskanta saboda shine mafi yawan uzuri kuma mafi gafara. Tagullar da aka narke daga amsawar zafi ta waje tana da kusan 1,083 °C - wurin narkewar tagulla - kuma da zarar ta haɗu da kowace ruwa, wannan ruwan yana tafasa zuwa tururi kuma yana faɗaɗa da kusan sau 1,700 a girma. Tururin yana juyawa ta cikin ƙarfen walda da aka narke, yana barin ramuka masu fashewa, kuma haɗin yana lalacewa kafin ya huce.Binciken abubuwan da suka faru na OSHA kan ayyukan walda mai zafi, wannan tsari guda ɗaya ya haifar da ƙarin raunukan ƙonewa da ƙonewar ma'aikatan jirgin sama fiye da kowace kuskuren tsarin exothermic.

Dalilin da ya sa hakan ya gaza a hankali shi ne cewa danshi yana da wurare uku na ɓuya, kuma ɗaya ne kawai daga cikinsu a bayyane yake.

Amsa Nugget:Lalacewar walda ta waje da danshi ba ta faruwa ne sakamakon ruwan da ba za a iya gani ba - ruwan da ba za a iya gani ba ne ke haifar da shi, kuma gwajin filin yana aiki ne ta hanyar injiniya, ba ta hanyar gani ba. Saboda foda yana shan danshi ba tare da gani ba, abin da kawai za a iya tabbatarwa shi ne: samfurin foda da aka busar da shi wanda ke zuba cikin 'yanci, mai gogewa da kyalle mai tsabta wanda ya fita ba tare da duhu ba, da kuma mold da aka riga aka dumama zuwa akalla digiri 30 na Celsius kafin ya taɓa mai sarrafa.

Gawar Cebu a layi uku

Haɗaɗɗun Cebu sun lalace saboda foda ya zauna a kan wani tashar jiragen ruwa da ruwan sama ya jika, kuma ma'aikatan jirgin sun buɗe gwangwani da safiyar ranar da aka zuba ruwan. Sun yi amfani da foda ɗin ko ta yaya domin ya yi kama da bushe - kuma ƙasan dutsen, a kan kowace haɗin gwiwa da ya lalace, ya nuna ainihin tsarin bututun iska da tururi mai danshi ke bari a baya. Duba na'urar busar da kaya ta minti 20 a kan kwalaye uku kafin zubar ruwan zai kama dukkan rukunin, kuma ma'aikatan jirgin sun san za su killace sauran.

Shin Mold ɗin Graphite ɗinku ya lalace bayan Tagar Sabis ɗinsa ta Gaskiya?

Wannan shine dalilin da ya sa masu samar da kayayyaki ke magance matsalar, saboda yanayin gazawar ba ya ganuwa ga mai siye kuma adadin zagayowar wani abu ne da mai samar da kayayyaki kawai ya sani.Littattafan samfurin Cadweld na nVent ERICOyana ƙididdige ƙirar graphite a kusan zagayowar sabis na 50 zuwa 100, kuma akan layinmu muna ƙididdige ƙimar namumold ɗin walda mai zafia zagaye 50 zuwa 100 iri ɗaya, tare da haɗin gwiwa 80 zuwa 100 a amfani da filin a al'ada. Bayan haka, ramin ya lalace sosai har ramin famfo bai ƙara auna ƙarfe mai narkewa cikin haɗin ba.

Alamar gaskiya ta mold da ya lalace ba tsagewa ba ce da za ku iya gani - dutsen walda ne da ya rasa siffar matashin kai kuma ya fara shiga ciki a tsakiya. Sabuwar mold tana samar da dutsen da ke lulluɓe a hankali a kan mai jagoranci, saboda cajin foda yana cika ramin da yawan walda a cikin mai hawan. Mold da ya lalace yana cika ƙasa, saboda ramin ya faɗaɗa sosai har cajin foda ɗaya ba ya da ƙarin da ya wuce kumfa. Ma'aikatan suna ramawa ta hanyar ƙara foda, wanda daga nan zai yi zafi fiye da kima kuma ya hanzarta lalacewa - madauri mai amsawa wanda ke ɗaukar kimanin zubar da mummunan abu ashirin don lalata mold gaba ɗaya.

Yadda ake kimanta siffar da ba ku saya daga gare mu ba

Idan ka gaji molds daga wani mai samar da kayayyaki, ka auna ɗaya da wani mold da aka sani mai siffar iri ɗaya. Mold graphite yana rasa kimanin gram 3 zuwa 8 a kowace zagaye sakamakon zaftarewar zafi da tsaftacewa; mold mai gram 50 a ƙarƙashin nauyinsa na farko yana da zagayowar fiye da yadda ƙimarsa ta yarda. Na biyu, duba siffar beads ɗin walda a cikin zubar biyar na ƙarshe - idan akwai ɗaya daga cikinsu a ciki, mold ɗin an tura shi ta hanyar taga mai kyau.IEEE Std 837-2014, tsarin cancantar haɗin ƙasa na dindindin na ƙarƙashin ƙasa, yanayin ramin walda wani ɓangare ne na shaidar cancantar - don haka mold ɗin da ya lalace ba wai kawai haɗarin inganci bane, haɗarin bin ƙa'ida ne akan mizanin da aka ƙayyade haɗin.

Shin ƙaramin girman foda zai iya rage ƙarfin walda a cikin na'urarka?

Foda tana zuwa a cikin girman harsashi na yau da kullun saboda dalili.Saboda rabon foda-da-jan ƙarfe shine canjin da ke tantance ko amsawar ta samar da isasshen zafi don narke sashin haɗin gwiwar mai gudanarwa gaba ɗaya, rage girman harsashin yana ƙirƙirar haɗin gwiwa wanda ke zuba danshi a waje amma ba a haɗa shi sosai a mahaɗin mai gudanarwa ba.Dutsen ya yi kyau sosai. Juriyar ta faɗi gaskiya watanni shida bayan haka lokacin da haɗin ya yi zafi a ƙarƙashin wutar lantarki ta farko.

Gaskiyar magana game da wannan gazawar ita ce ma'aikata kan maye gurbin ƙaramin harsashi idan girman da ya dace ya ƙare, bisa ga zato cewa "ƙarfe ɗaya ne ko ƙasa da haka". Sigar rashin gaskiya ita ce wasu masu samar da kayayyaki za su sayar da harsashi #115 a farashin #150 saboda fom ɗin odar ɗan kwangilar ya ce "kebul-zuwa-kebul 50 mm²" ba tare da bayyana cikakken haɗin jagora ba. Dukansu suna ƙarewa da haɗin gwiwa iri ɗaya: kyakkyawan dutsen dutse, ƙaramin rami a cikin mai jagoran, da juriya da ke raguwa kowace shekara.

Amsa Nugget:Girman foda ba shawara ce ta farashi ba — shawara ce ta zafi-matsakaici. Domin kuwa amsawar zafin jiki dole ne ta fitar da isasshen kuzari don dumama sashin haɗin gwiwar mai jagora sama da wurin narkewar jan ƙarfe (1,083 °C) kuma ta ci gaba da narkewa har tsawon lokacin da za a iya haɗa shi, harsashin da ba shi da girman da ya dace da na'urar haɗin gwiwa yana barin mafi zurfin zaren mai jagora ƙasa da zafin haɗuwa. Koyaushe daidaita harsashin da babban mai gudanarwa biyu, ba ƙarami ba.

Shin gajerun hanyoyin shirya na'urar jagora sune ɓoyayyen sanadin haɗin gwiwa masu juriya sosai?

Na kalli ma'aikata suna shafe mintuna ashirin suna tsaftace ɓangaren da ake iya gani na zaren tagulla kuma suna tsallake ɓangaren da ke shiga cikin ramin mold, saboda takardar bayanin ta ce "mai tsabta zuwa ƙarfe mai haske" ba tare da bayyana yadda za a yi ba.Saboda haɗin yana samuwa a saman jagoran da ke cikin ramin a lokacin da aka zuba shi, wani ɓangare mai gurɓataccen abu a ƙarƙashin ramin yana ƙirƙirar haɗin gwiwa wanda yake ci gaba da aiki a waje kuma an yi masa laminated da oxide a ciki.

Gurɓataccen gurɓataccen da na gani a binciken da aka yi a kan na'urorin bincike ba datti ba ne - shine yatsan hannu. Ma'aikatan suna kula da sashin jagoran da ke shiga cikin mold ɗin, suna barin siririn fim ɗin mai daga fatarsu, kuma jan ƙarfe mai narkewa ba zai iya jika ta cikin fim ɗin don haɗawa da ƙarfen tushe ba. Sakamakon shine haɗin gwiwa tare da jirgin oxide mai ci gaba tsakanin ƙarfe na walda da mai jagora, kuma jirgin oxide shine ainihin nau'in haɗin da NUREG-1800 ke ɗauka a matsayin hanyar lalata a ƙarƙashin zagayowar zafi.

Shin Lokacin Kunna Mold Mai Sanyi Yana Haifar da Kuskuren Aikin Safiya?

Wannan shine dalilin da yasa babu wanda ya rubuta, domin yana kama da kuskuren mai aiki maimakon kuskuren tsari. Gaskiyar magana ita ce amsawar exothermic ana daidaita ta zuwa wani takamaiman ambulan zafi, kuma mold wanda yake ƙasa da 25 °C a lokacin kunna wuta yana aiki daban da wanda aka riga aka dumama shi. Foda mai farawa yana ƙonewa, gaban amsawar yana yaɗuwa ta hanyar caji, amma jan ƙarfe mai narkewa yana rasa zafi zuwa graphite mai sanyi da sauri fiye da yadda amsawar zata iya sake cika shi, kuma ƙarfen yana isa ramin mai gudanarwa a ƙasa da zafin haɗuwa. Har yanzu bead ɗin yana samuwa. Haɗawar ba ta cika ba.

Wannan matsala ce ta aiki da safe a wurare masu zafi ko sanyi, kuma babbar matsala ce ta aiki da rana a wurare masu zafi inda ma'aikata ke sanyaya injinansu kafin su sanyaya a cikin wurin ajiyar iska don "kiyaye su". Kowace dabi'a tana haifar da irin wannan yanayin rashin aiki: layin rufewa da sanyi inda bangarorin ƙarfe biyu suka haɗu amma ba su haɗu sosai ba, wanda ake iya gani a kan giciye a matsayin katsewa mai kaifi a cikin tsarin hatsi a daidai da bangon rami.

Amsa Nugget:Zafin mold a lokacin kunna wuta abu ne mai matuƙar canzawa, ba abin da ake so ba. Saboda graphite yana gudanar da zafi a hankali, mold da aka adana a ƙasa da 25 °C yana buƙatar ɗumi mai aiki - mintuna biyar tare da bindiga mai zafi mai ƙarancin zafi, mintuna goma a zaune a kan murfin injin mai ɗumi, ko kuma kawai a ajiye shi cikin dare a cikin iska iri ɗaya da zubar da ruwa. Dumama kafin zuwa 30-40 °C yana kawar da yanayin lalacewar sanyi ba tare da shafar rayuwar mold ba.

Jerin Binciken Bincike: Abin da za a yi idan Haɗin gwiwa ya gaza Aiki

Idan haɗin gwiwa ya gaza aiwatar da aiki, a gudanar da binciken kamar haka. Dubawa uku na farko suna ɗaukar ƙasa da awa ɗaya a wurin kuma suna warware kusan kashi 80% na gazawar haɗin gwiwa da yawa ba tare da yanke komai ba.

  1. Tabbatar da tarihin tarin foda.Yaushe aka kawo foda, ta yaya aka adana shi, kuma an buɗe wasu gwangwani kafin a zuba? Duk wani amsar "eh" yana nuna danshi (Dalilin 1).
  2. Ja log ɗin mold ɗin.Dawaki nawa ne mold ɗin ya yi? Ma'anar da aka yi amfani da ita idan aka kwatanta da ma'aunin zagayowar 50-100. Duk wani mold da ya wuce ma'auninsa za a maye gurbinsa kafin a zuba na gaba (Dalilin 2).
  3. Duba girman foda a kan jadawalin jagora.Daidaita girman harsashin a kowace gwangwani da haɗin mai jagora a kan haɗin. Ana sake zuba rashin daidaiton da harsashin da ya dace (Dalilin 3).
  4. Duba haɗin gwiwa guda uku da suka lalace a kan sashe na giciye.Yanke sandunan ƙarfe da gogewa ya isa ya gano tsarin ramuka masu busawa (Dalilin 1), lamination na oxide (Dalilin 4), cika ƙasa (Dalilai 2 da 3), ko layukan rufe sanyi (Dalilin 5).
  5. Taswirar gazawa akan jerin zubarwa.Kurakuran da aka tara a farkon canji kusan koyaushe suna nuna Sanadin 5 (sanyi mold). Kurakuran da aka tara a ƙarshen wurin foda zuwa Sanadin 1 (jika foda). Kurakuran da aka tara sun bazu ko'ina a kan wurin canzawa zuwa Sanadin 2 ko 4.

Idan gazawar ta wuce dukkan gwaje-gwaje guda biyar, to tabbas matsalar ta shafi muhalli ne - sinadaran ƙasa, kwararar ruwa, ko kuma tsatsa ta galvanic da ke gano hanyar haɗin da walda ta bari - kuma dole ne tattaunawar ta canza daga tsari zuwa tsari. Wannan tattaunawar ita ce labarinta.

Sake Zuba Da'a: Ragewa, Ba Sake Wanka a Wurinsa Ba

Da zarar haɗin gwiwa ya lalace, gyara ɗaya tilo da ya dace shine a yanke gefen da zafi ya shafa sannan a sake shirya mai jagoran daga farko. Zuba sabon ƙarfe na walda a kan haɗin da ya lalace ba ya haɗa sabon ƙarfe zuwa tsohon amintacce, saboda asalin haɗin ya riga ya samar da nasa ƙarfe kuma duk wani rami da ya makale ya zama wurin nucleation don gazawar gaba. Ya kamata a yanke ƙarshen ya zama aƙalla mm 50 na mai jagoran tsabta a kowane gefen haɗin farko, sabon ƙirar ya kamata ya kasance a cikin adadin zagayowarsa, kuma ya kamata a yi amfani da foda daga gwangwani da aka buɗe, wanda aka tabbatar da busasshe.

Zubar da mold a karo na biyu kuma shine lokacin da ya dace don haɓaka mold ɗin idan gazawar ta nuna lalacewar mold. Muna jigilar namu.mold ɗin walda na wajetare da rajistar zagayowar da aka tsara don masu siye su iya bin diddigin tarihin kowace mold a cikin wani aiki, kuma rajistar iri ɗaya ya kamata ta yi tafiya tare da kowace mold da ke motsawa tsakanin shafuka. Mold ɗin da ba za ku iya lissafa shi ba mold ne da ba za ku iya amincewa da shi ba.

Dalilai biyar, duba filin wasa biyar, mintuna biyar a kowace haɗin gwiwa
Dalili Abin da za a tabbatar a shafin Lokaci a kowace haɗin gwiwa
Danshi Gwajin bushewa a kan harsashin samfurin; gwajin gogewa na jagora; zafin saman mold ≥ 30 °C Minti 2
Lalacewar mold Rigon zagayowar mold; siffar beads a cikin zubarwa biyar na ƙarshe; nauyin mold vs nauyin farawa Minti 1
Foda mara girman girma Jadawalin girman harsashi da na'urar jagoranci; duba ingancin rukuni Minti 1
Shiri na jagorar jagora Duba ƙarfe mai haske; babu taɓawa a fata bayan tsaftacewa; ≤ minti 15 a buɗe tagar Minti 1
Sanyi kunna wuta Ana iya dumama shi kafin a kunna shi idan ƙasa da 25 °C; a yi amfani da ma'aunin zafi na infrared ko ma'aunin zafi na lamba kafin a kunna shi. 30s

Yadda Ake Duba Mai Ba Kayayyakinka Na Yanzu Ba Tare Da Cin Zarafin Kowa Ba

Yawancin kiran da nake yi kan wannan batu ba sa farawa da gazawa. Suna farawa da mai siye wanda aka nemi ya cancanci sabon mai samar da kayayyaki, ko injiniya wanda ya gaji wani tsari da bai tsara ba, kuma suna son sanin tambayoyin da za su yi kafin gazawar ta gaba. Gaskiyar magana ita ce kusan kowace mai samar da kayayyaki za ta iya aika da wani tsari da ke aiki a ranar da aka fara amfani da shi. Tambaya mafi wahala ita ce ko za su iya rubuta dalilin da ya sa samfurinsu ya yi aiki, da kuma ko za su mallaki amsar idan ba ta yi ba.

Tambayoyi uku sun bambanta mai samar da kayayyaki na gaske da mai rage farashi akan wannan takamaiman matsalar, kuma zan yi wa kowane mai siye bayani ta wannan tsari.

  1. "Nuna min samfurin rajistar zagayowar mold ɗinka."Mai samar da kayayyaki wanda ke bin diddigin adadin zagayowar kayayyaki ne wanda ya san cewa molds yana lalacewa. Mai samar da kayayyaki wanda bai yi ba, ba shi da kyau ya kawar da matsalar da ke tattare da su.
  2. "Menene ma'aunin gano foda ɗinka?"Kowace gwangwani ya kamata ta ƙunshi lambar batch, ranar da aka ƙera ta, da kuma alamar kwantena da aka rufe. Mai samar da kayayyaki wanda ya sake tattara foda mai yawa zuwa gwangwani wanda ba a yiwa alama ba yana da haɗarin danshi a cikin gwangwani.
  3. "Menene matsayinka game da maye gurbin ƙaramin harsashi?"Amsar gaskiya ita ce "ba za mu ƙi odar ba har sai kun tabbatar da girman na'urar jagora." Amsar mai haɗari ita ce "za mu iya aika ƙaramin gwangwani a yau."

Mun gina takardun fitar da kayayyaki zuwa ƙasashen waje bisa ga waɗannan tambayoyi uku domin su ne tambayoyin da binciken gazawarmu ke ci gaba da mayar da hankali a kansu. Su ne kuma tambayoyin da zan yi mana, idan ni mai siye ne.

Ganewar Rashin Nasarar Walda — Zaɓi Alamar da Kake Gani a Fagen

Kafin ka yanke haɗin gwiwa ɗaya, gudanar da wannan bincike. Zaɓi alamar da ta yi daidai da abin da kake gani a wurin - na gani, na lantarki, ko tsarin lokaci - sannan kayan aikin ya mayar da shi zuwa ga mafi kusantar dalilai biyar da ke sama, yana ba ka kwarin gwiwa, kuma ya lissafa matakan da za a ɗauka nan take kafin a sake zuba. Wannan ita ce hanya ɗaya tilo da nake bi wajen tuntubar mai siye ta waya idan kiran da ya gaza ya shigo.


Mafi yuwuwar dalili
Dalili na 3 — Ƙaramin cajin foda (wanda aka fi sani da shi), ko kuma kuskuren tsari na mold lokacin rufewa
Kwarin gwiwa
Matsakaici - yana tabbatar da rashin cikar zuba amma ba zai iya bambance daidaiton foda da mold ba tare da dubawa ba
Matakan kulawa nan take
  1. Tabbatar da girman harsashin a kan haɗin mai gudanarwa - ƙaramin caji shine babban dalilin da ya sa ba a cika haɗa shi da mai gudanarwa ɗaya ba.
  2. Duba daidaiton mold: dole ne rabi biyu su rufe a tsakiyar layin jagora ba tare da hasken rana ya bayyana ba.
  3. Duba faifan ƙarfe - dole ne ya zauna a tsakiya a kan ramin famfo kafin a kunna shi, ba a taɓa motsa shi daga axis ba.
  4. Sake shirya na'urar kwandishan da sabon goga da kuma gogewar isopropyl kafin a zuba na gaba.
  5. Yi hoton haɗin da ya lalace da kuma daidaitawa kafin a cire shi don a iya duba na gaba a kan na'urar.
Nassoshi
Duba 'Shin Cajin Foda Mai Ƙaranci Zai Iya Rage Walda a Hankali?' a sama.

Binciken ya nuna wata alama guda ɗaya da ta fi yiwuwa ta samo asali ne daga kurakurai 312 da aka rubuta a masana'antarmu tsakanin 2023 da 2026. Idan alamu biyu suka yi karo, a yi amfani da na biyu daban-daban - za su nuna tushen wannan matsalar a kusan kashi 80% na shari'o'in da suka shafi mahaɗi.

Tambayoyin da Ake Yawan Yi Game da Rashin Nasarar Walda Mai Tsami

Ta yaya zan sani idan walda ta exothermic ta gaza idan har yanzu tana da ƙarfi?

Weld ɗin thermit da ya gaza zai iya yin kyau a waje kuma har yanzu yana da mummunan haɗin gwiwa. Alamun da aka dogara da su na lantarki ne: karatun juriyar milliohm wanda ke hawa shekara bayan shekara, hoton zafi da aka ɗauka a ƙarƙashin kaya wanda ke nuna haɗin yana aiki fiye da mai jagoran, ko kuma zoben jan ƙarfe mai launin kore a wurin fita daga mai jagoran. Duba gani kaɗai yana kama mafi munin gazawa kawai - porosity da ya fashe ta saman ko kuma wani cika da ya ɓace a ramin famfo.

Za a iya sake haɗa walda mai zafi ta waje a wurin da ba ta yi aiki ba, ko kuma dole ne a yanke wa mai tuƙi?

Dole ne ka yanke bayan yankin da zafi ya shafa sannan ka sake shirya sabon mai jagoranci. Zuba sabon ƙarfe a kan haɗin da ya lalace ba ya haɗa sabon ƙarfe zuwa tsohon tagulla da aminci saboda asalin haɗin ya riga ya samar da nasa ƙarfe kuma duk wani rami da ya makale ya zama wurin nucleation don gazawar gaba. A aikace, haɗin da ya gaza yana nufin rage aƙalla mm 50 na mai jagoranci a kowane gefe, tsaftacewa zuwa ƙarfe mai haske, da amfani da sabon mold na graphite - kuma sai bayan ka gano tushen abin da ya jawo hakan.

Menene danshi yake yi a cikin walda mai zafi?

Tagullar da aka narke daga amsawar zafi ta waje tana da zafin da ya kai kimanin digiri 1,083 na Celsius, kuma duk wani ruwa da ya makale a cikin ramin mold, a kan mai sarrafa wutar lantarki, ko kuma a cikin walƙiyar foda yana haskakawa don tururi da zarar ƙarfen ya iso. Tururin yana faɗaɗa kusan sau 1,700 a girma kuma yana fitar da ƙarfi ta cikin ƙarfen walda da aka narke, yana barin ramuka masu busawa da haɗin da aka yi da oxide. A cikin mafi munin yanayi, fashewar tururin ta jefa ƙarfe mai narkewa daga cikin abin da ke kewaye da shi da kuma ƙonewa - wannan shine rikodin raunin OSHA da aka fi sani akan ayyukan walda mai zafi.

Har yaushe ya kamata a yi amfani da mold ɗin walda na graphite exothermic?

A layinmu, muna ƙididdige molds na graphite a zagayen sabis na 50 zuwa 100, da kuma haɗin gwiwa 80 zuwa 100 a amfani da filin na yau da kullun, saboda kowanne zuba yana lalata ramin kuma yana faɗaɗa ramin famfo a hankali. Mold da aka tura fiye da adadin zagayowarsa yana fara samar da haɗin gwiwa da ba a cika ba, kuma masu aiki suna ramawa ta hanyar ƙara foda - wanda daga nan yana dumama ramin kuma yana hanzarta lalacewa. Siginar gaskiya ba tsagewa ba ce da za ku iya gani; shine bead ɗin walda yana rasa siffar matashin kai na musamman kuma yana fara narkewa a ciki.

Me yasa walda ta exothermic ɗina take da kyau amma tana auna juriya mai yawa lokacin da aka yi mata aiki?

Babban juriya akan walda wanda yayi kama da daidai kusan koyaushe yana komawa ga ɗaya daga cikin abubuwa uku: ba a tsaftace mai jagora zuwa ƙarfe mai haske a ƙarƙashin ramin walda ba, ƙimar foda ta kasance ƙasa da girman giciye na mai jagoran, ko kuma an daidaita mold ɗin ba daidai ba don haka ƙarfen da aka narke ya haɗu da masu jagoranci maimakon haɗawa cikin duka biyun. Kyakkyawan walda da walda mai ƙarancin juriya ba abu ɗaya bane ta atomatik, saboda ana ɗaukar ma'aunin juriya a kan haɗin gwiwa, ba ta cikin dutsen ba. Mun ga haɗin gwiwa masu kyawawan beads suna auna micro-ohm 800 akan micro-ohm mai lafiya 30 zuwa 50 akan maƙwabta iri ɗaya.

Menene bambanci tsakanin gazawar walda ta waje da kuma gazawar walda tun daga farko?

Lalacewar walda ta waje (exothermic weld) wani haɗin gwiwa ne da ke aiki daidai lokacin shigarwa sannan ya lalace yayin aiki - yawanci ta hanyar tsatsa a mahaɗin jagora, walda ba ta taɓa kaiwa ba, ta hanyar zagayowar zafi wanda ya buɗe ƙaramin rami, ko ta hanyar matsala ta injiniya. Walda mai lahani ba ta taɓa yin kyau ba: an zuba shi da foda mai jika, babban rami, mold da ya lalace, ko kuma gurɓataccen mai jagora, kuma gazawar tana bayyana a lokacin aiki ko gwajin kaya na farko. Bambancin al'amura biyu saboda gazawa sau da yawa yana nuna matsalar muhalli, yayin da lahani ke nuna matsalar tsari ko mai samar da kayayyaki.

Jane Yang· Manajan Talla, Xinchang Shibang New Material Co., Ltd.
Shekaru 12 a fannin kare walƙiya da kuma dakatar da cinikin ƙasashen waje · Shekaru 17 na samar da masana'antu bayan kowace shawara.
LinkedIn · Facebook · X


Lokacin Saƙo: Agusta-27-2026