- Ƙasa mai gurɓatawa tana lalata sandunan ƙasa marasa inganci cikin watanni, ba shekaru da yawa ba
- Kauri mai kauri a cikin ruwan zafi yana ƙayyade tsawon rayuwar sandar a cikin ƙasa mai ƙarfi
- Ƙasa mai arzikin chlorine a bakin teku da kuma ƙasa mai tsami tana buƙatar ƙarin nauyin sinadarin zinc
- Sandunan lantarki masu rahusa suna rasa kariya sau 3 zuwa 5 cikin sauri fiye da nau'ikan tsoma-zafi.
- Gwajin ƙasa mai kyau kafin ƙayyadewa yana hana maye gurbin gona mai tsada
- Zurfin shigarwa da kayan cikawa suna faɗaɗa ko rage tsawon rayuwar sabis na sandar
- Sandunan ƙarfe masu lulluɓe da na tagulla sun dace da yanayi mafi tsauri inda samfuran galvanized suka kai iyaka
Teburin Abubuwan da ke Ciki
- Dalilin da Yasa Ƙasa Mai Lalacewa Ke Rusa Sandunan Ƙasa Masu Sauri Fiye da Yadda Kuke Tsammani
- Me Yake Sa Ƙasa Ta Yi Lalata? pH, Juriya, da Sinadaran
- Yadda Zafi-Tsaftace Galvanization Ke Kare Zuciyar Karfe (da Kuma Inda Yake Faɗuwa)
- Gaskiyar Kudin Da Aka Kashe Na Rashin Aikin Sanda A Fili
- Yadda Ake Bayyana Sandar Ƙasa Mai Daidaita Gaske Don Ƙasa Mai Lalacewa
- Ayyukan Shigarwa Waɗanda Ke Fadada Tsawon Rayuwar Sandar Ƙasa
- Lokacin da za a Haɓaka: Madadin Rufin Tagulla ko Bakin Karfe
- An lulluɓe da ƙarfe mai kauri da ƙarfe mai kauri da ƙarfe mai kauri: Kwatanta Gefe-da-Gefe
- Tambayoyin da Ake Yawan Yi Game da Lalata Sanda Mai Gina Ƙasa
Dalilin da Yasa Ƙasa Mai Lalacewa Ke Rusa Sandunan Ƙasa Masu Sauri Fiye da Yadda Kuke Tsammani
Yaushelalata sandar ƙasa ta galvanizedyana bayyana a wurin aiki, tushen matsalar kusan koyaushe yana komawa ga shawarar siye wanda muke gani sau da yawa wanda ya fifita mafi ƙarancin farashin naúrar fiye da dacewa da kayan. Muna ganin wannan tsari akai-akai a masana'antarmu: ɗan kwangila yana yin odar sandunan da ake da su mafi arha daga mai samar da kayayyaki masu araha, yana sanya su a cikin ƙasa mai wahala ba tare da jagorarmu ba, sannan ya tuntube mu bayan shekaru biyu ko uku yana tambayar mu dalilin da yasa suketsarin ƙasa ya gazagwajin impedance.
Injiniyoyinmu sun bayyana cewa rufin zinc da ke kan sandar ƙasa mai galvanized yana aiki a matsayin anode na hadaya. Yana yin laushi sosai, yana kare tsakiyar ƙarfe da ke ƙasa. Da zarar an cinye layin zinc, ƙarfe mara komai yana yin lalacewa da sauri kuma sandar ta rasa daidaiton tsarinta da kuma hulɗar wutar lantarki da ƙasar da ke kewaye. A cikin yanayin ƙasa mai laushi tare da pH mai tsaka-tsaki da ƙarancin danshi, sandunan galvanized da muke tsomawa a cikin zafi na iya ɗaukar shekaru 20 zuwa 30.lalata ƙasaaikace-aikace, wannan lokacin ya ruguje sosai.
Za mu iya nuna wani wurin da aka gina a bakin teku a yankin Tekun Fasha wanda ya nuna wannan a sarari. Ƙasa a yawancin gabar tekun UAE da Saudiyya tana ɗauke da sinadarin chloride da sulfates masu yawa, tare da ƙimar juriya mai ƙasa da santimita 200. A ƙarƙashin waɗannan yanayi, mun lura cewa sandar da aka yi da sirara mai rufi da electro-galvanized ta rasa kariyar zinc cikin shekaru 3 zuwa 5. Sannan tsakiyar ƙarfen yana lalacewa a cikin mililita 0.5 zuwa 1.0 a kowace shekara, wanda hakan ke haifar da kammalawa.gazawar sandar ƙasaTun kafin kayayyakin more rayuwa su kare, kamfanin ya kai ƙarshen rayuwarsa. Ɗan kwangilar da ya adana kuɗi kaɗan a kowace sanda yanzu yana fuskantar kuɗaɗen tara kuɗi, haƙa rami, sake tuƙi, da sake gwadawa wanda ya ninka farashin siyan farko.
Ƙungiyar injiniyancinmu ta rubuta irin wannan sakamako a duk faɗin yankin kudu maso gabashin Asiya mai zafi, kuma muna raba waɗannan binciken ga abokan cinikinmu, inda ƙasa mai acidic laterite tare da ƙimar pH tsakanin 3.8 da 5.0 ke narkar da rufin zinc a cikin sauri. Ayyukan da aka yi a Malaysia, Indonesia, da Philippines waɗanda suka ƙayyade sandunan galvanized na yau da kullun ba tare da la'akari da acidity na ƙasa ba sun buƙaci maye gurbin sandar cikin shekaru 5 zuwa 8. Mun ga wannan tsari yana maimaitawa a cikin yankuna da nau'ikan ƙasa, kuma ƙarshenmu ya kasance iri ɗaya: mafi arha ƙimar yana haifar da gazawar mafi tsada lokacin da ƙayyadaddun sandar bai dace da yanayin wurin ba.
Me Yake Sa Ƙasa Ta Yi Lalata? pH, Juriya, da Sinadaran
Lalacewar ƙasa ba abu ɗaya da za a iya aunawa ba ne. Yana fitowa ne daga haɗakar tasirin abubuwa da sinadarai da yawa waɗanda suka bambanta da zurfin, yanayi, da wurin da ake. Muna taimaka wa injiniyoyi da masu ƙayyadewa su fahimci waɗannan abubuwan don su iya zaɓar abin da ya dace.sandar ƙasa ta galvanizedga kowane shafin yanar gizo da aka bayar.
Matsayin Narkewar Zinc da pH na ƙasa
matakin pHyana kula da yanayin sinadarai da ke kewaye da sandar. Ƙasa mai acidic tare da pH ƙasa da 5.5 tana narkar da zinc ta hanyar kai tsaye hari kan sinadarai, tana samar da gishirin zinc mai narkewa wanda ke wankewa da fallasa sabon ƙarfe ga ƙarin tsatsa. Ƙasa mai alkaline tare da pH sama da 9.0 tana samar da layin zinc oxide mai aiki wanda ke tsayayya da tsatsa, amma kasancewar yawan carbonate ko ammonia a cikin ƙasa mai alkaline na iya lalata wannan kariyar. Mun gano cewa ƙasa mai tsaka-tsaki (pH 6.0 zuwa 8.0) tana samar da yanayi mafi laushi ga rufin zinc ɗinmu.
Juriyar Ƙasa da Yawan Tsatsa
Juriyar ƙasayana auna ikon ƙasa na gudanar da wutar lantarki kuma yana da alaƙa da yawan danshi da kuma yawan ion da ya narke. Ƙananan juriya (ƙasa da santimita 1000 ohm) suna nuna babban danshi da gishirin da ya narke, waɗanda duka suna hanzarta lalata sandar ƙasa mai galvanized. Babban juriya (sama da santimita 5000 ohm) yana nuna busasshiyar ƙasa, yashi, ko dutse inda tsatsa ke ci gaba a hankali. Muna amfani daMatsayin ASTM G57, wanda ke bayyana hanyar Wenner mai fil huɗu wadda ta kasance mizanin masana'antu don auna juriyar filin, kuma muna ba da shawarar abokan cinikinmu su bi ta.
Chloride, Sulfate, da kuma Haɗarin Acid na Halitta
Sinadarin sinadaraiyana kammala hoton. Ion ɗin Chloride suna kai hari ga rufin zinc kai tsaye, suna haifar da tsatsa mai zurfi wanda ke ratsa layin zinc a wurare daban-daban kuma ya isa tsakiyar ƙarfe da sauri fiye da tsatsa mai kama da juna. Kwayoyin cuta masu rage sulfate a cikin ƙasa mai cike da ruwa suna samar da hydrogen sulfide, wanda ke amsawa da zinc don samar da zinc sulfide, wani sinadari mara kariya. Acid na halitta a cikin ƙasa mai arzikin peat da humus yana narkar da zinc ta hanyar chelation, kuma mun yi la'akari da wannan a cikin shawarwarinmu. Ƙungiyarmu a Shibang tana tantance bayanan sunadarai na ƙasa daga wuraren abokin ciniki don daidaita ƙayyadaddun murfin sandarmu zuwa ainihin barazanar tsatsa. Ba mu yarda da dogaro da zato ɗaya-girma-ya dace da kowa ba saboda ƙwarewarmu ta nuna cewa kowane wuri ya bambanta.
Bayanin Injiniya:A yankunan arewacin Turai na permafrost, zagayowar daskarewa da narkewa yana gabatar da ƙarin hanyar tsatsa. Yayin da ruwan ƙasa ke daskarewa da faɗaɗa, yana haifar da matsin lamba na injiniya a saman sandar wanda zai iya fasa layin zinc. Lokacin da ƙasa ta narke, danshi yana ratsa waɗannan ƙananan fasa kuma yana hanzarta tsatsa ta gida. Ayyuka a Finland, Norway, da arewacin Kanada suna buƙatar sanduna masu kauri da rufin zinc da hanyoyin tuƙi masu sassauƙa don guje wa tsatsa layin galvanized yayin shigarwa a cikin ƙasa mai daskarewa kaɗan.
Yadda Zafi-Tsaftace Galvanization Ke Kare Zuciyar Karfe (da Kuma Inda Yake Faɗuwa)
Yin amfani da galvanization mai zafi yana haifar da haɗin ƙarfe tsakanin zinc da ƙarfe ta hanyar nutsar da sandar ƙarfe da aka shirya a cikin wanka na zinc mai narkewa a kimanin digiri 450 na Celsius. Tsarin yana samar da tsarin rufewa mai layuka da yawa: Layer na waje na zinc mai tsarki, matakan ƙarfe na zinc-iron matsakaici, da kuma substrate na ƙarfe. Muna jaddada wannan tsari saboda yana da mahimmanci ga juriyar tsatsa: yadudduka na ƙarfe suna da ƙarfi kuma sun fi juriya ga tsatsa fiye da zinc mai tsarki kaɗai, shi ya sa sandunanmu suka fi sirara madadin lantarki mai galvanized.
Ma'aunin Nauyin Rufi da Tsarin Samarwa namu
A masana'antarmu, muna bin diddiginsandar ƙasa mai zafi da aka yi da galvanizedKa'idojin samarwa waɗanda ke isar da nauyin rufi na 550 g/m2 ko sama da haka, tare da kauri na yau da kullun na microns 70 zuwa 80. Wannan yana wakiltar babban ci gaba akan rufin da aka yi da electro-galvanized, wanda yawanci ya kama daga microns 5 zuwa 15. Mun ga babban bambanci a cikinRayuwar sandar ƙasa ta galvanizedtsakanin waɗannan matakai guda biyu: sandunan mu na tsoma zafi akai-akai suna ba da sabis na shekaru 15 zuwa 25 a cikin ƙasa mai laushi, yayin da sandunan da aka yi amfani da wutar lantarki a cikin ƙasa ɗaya ke kaiwa ƙarshen rayuwa cikin shekaru 3 zuwa 7.
Tsarin Anode na Zinc
Tsarin kariya daga hadaya yana aiki ta hanyar aikin lantarki. Zinc yana da ƙarfin lantarki mai rauni fiye da ƙarfe, don haka idan ƙarfe biyu suna cikin electrolyte (ƙasa mai danshi), zinc yana yin tsatsa kuma ƙarfen yana kasancewa mai kariya ta cathod.Tasirin anode na hadayayana kare ƙarfen ko da a ƙananan ƙagaggunan ko bukukuwa a cikin rufin zinc, wanda babban fa'ida ne akan rufin shinge kawai kamar fenti ko epoxy.
Mun bayyana a fili inda galvanization na tsoma zafi ya gaza, wanda yake a cikin mawuyacin yanayi. A cikin ƙasa mai yawan chloride sama da 500 ppm, pH ƙasa da 4.0, ko juriya a ƙasa da santimita 200 na ohm, har ma da kauri mai laushi na tsoma zafi yana ɓacewa da sauri. Sandar ƙasa mai kauri ta Q235 ɗinmu tana magance ƙalubalen tsatsa mai matsakaici yadda ya kamata, amma koyaushe muna gaya wa abokan cinikinmu da gaskiya: lokacin da bayanan ƙasa suka shiga cikin kewayon mai tsanani, sandunan jan ƙarfe ko bakin ƙarfe suna ba da tsawon rai na sabis. Amsar injiniyarmu ta gaskiya ita ce daidaita kayan sandar da tsananin tsatsa. Ba ma taɓa sayar da samfuran galvanized a cikin muhalli inda za su ba da kunya.
Gaskiyar Kudin Da Aka Kashe Na Rashin Aikin Sanda A Fili
Mun san hakangazawar sandar ƙasaBa kasafai ake samun labarai a kan labarai ba, amma sakamakonsa yana yaduwa ta hanyar kasafin kudin aikin, jadawali, da bayanan bin ka'idojin tsaro. Lokacin da tsarin saukar jiragen sama ya rasa takamaiman matakin hana shi, wurin da yake kare shi yana fuskantar karuwar hatsari daga bugun walƙiya, kwararar matsala, da kuma fitarwa mara motsi. Hukumomin da ke kula da harkokin tsaro a mafi yawan yankuna suna buƙatar takaddun ƙimar juriyar saukar jiragen sama, kuma gwajin da ya gaza yana haifar da gyara tilas.
Abokan cinikinmu sun gaya mana cewa farashin da ake kashewa kai tsaye wajen maye gurbin sandunan ƙasa da suka lalace sun haɗa da aikin haƙa ƙasa, sabbin siyan sanduna, haɗa kayan aikin tuƙi ko haƙa, da sake gwadawa. A cikin ƙwarewarmu ta tallafawa abokan ciniki na ƙasashen waje tare da manyan shigarwa, farashin maye gurbin kowace sanda ya kama daga sau 5 zuwa 15 na farashin siyan sanda na asali, ya danganta da damar shiga wurin da yanayin saman. Sandar da aka sanya a ƙarƙashin siminti ko saman kwalta tana buƙatar karyewa da sake zubawa, wanda hakan ke ƙara ninka farashin.
Mun gano cewa kuɗaɗen da ba na kai tsaye ba galibi sun fi na kai tsaye. Hasumiyar sadarwa da ta gaza binciken ƙasa na iya fuskantar umarnin rufewa har sai tsarin ya sake yin gwaji. Cibiyar bayanai da ta lalace sakamakon lalacewar ƙasa tana fuskantar ƙaruwar lalacewar kayan aiki sakamakon ƙarfin lantarki na ɗan lokaci. Masana'antar masana'antu da ba ta da isasshen tushe tana ganin ƙaruwar kurakuran kayan aiki da kuma matsalolin lantarki. Waɗannan katsewar aiki suna ɗaukar lokaci mai tsawo kuma suna da tsada fiye da maye gurbin sandar zahiri.
A Saudiyya, mun yi aiki kafada da kafada da wani dan kwangila wanda ya sanya sandunan lantarki masu amfani da wutar lantarki a wani gona mai amfani da hasken rana a cikin hamadar bakin teku ba tare da tuntubar tawagarmu ba tukuna. Cikin shekaru hudu, toshewar tsarin kasa ya tashi sama da iyaka saboda tsananinlalata sandar ƙasa ta galvanizedAikin maye gurbin ya buƙaci sake tattara ma'aikatan shigarwa, shigo da sabbin sanduna, da kuma tsara lokacin rufewa na kwanaki 10 wanda a lokacin da tsarin hasken rana ke aiki ba tare da cikakken kariyar girgiza ba. Jimillar kuɗin maye gurbin ya zarce kasafin kuɗin tushe na asali da kashi takwas. Mun gaya wa abokin ciniki cewa za a iya hana wannan sakamakon gaba ɗaya ta hanyar kimanta ƙasa da kuma ƙayyade yanayin da muke ciki.sandar ƙasa mai galvanizedtare da nauyin shafi mai dacewa tun daga farko.
Yadda Ake Bayyana Sandar Ƙasa Mai Daidaita Gaske Don Ƙasa Mai Lalacewa
Takamaiman sandun ƙasa masu galvanized don ƙasa mai lalata suna farawa da binciken wurin kuma suna ƙarewa da takardar siye wacce ke haɗa nauyin murfin sandar da ma'aunin ƙasa da aka auna. Ƙungiyarmu a Shibang tana bin tsarin da muka tsara tsawon shekaru 17 na samar da kayayyakinmu na ƙasa ga ayyukan ƙasa, kuma muna raba su a fili ga abokan cinikinmu.
Kimanta Ƙasa da Rarraba Tsatsa
Mataki na 1: Gwajin Ƙasa.Yi gwajin juriya a zurfafan wurare da yawa ta amfani da hanyar Wenner (ASTM G57). Tattara samfuran ƙasa a zurfin tuƙi na sandar da aka tsara don nazarin pH, chloride, sulfate, da acid na halitta a dakin gwaje-gwaje. Gwaji a yanayin busasshiyar damina idan wurin yana da yanayin ruwan sama ko lokacin damina.
Mataki na 2: Rarraba Tsatsa.Muna rarraba tsananin ƙasa ta amfani da ƙa'idodi da aka kafa.NACE ta Duniyayana ba da jagororin ta hanyar SP0169, yayin daIEC 62561Yana magance zaɓin sassan ƙasa. Ƙasa da aka sanya a matsayin mai lalata sosai tana buƙatar takamaiman sanda daban fiye da ƙasa mai ɗan lalata.
Zaɓin Nauyin Rufi da Diamita na Sanda
Mataki na 3: Zaɓin Nauyin Rufi.Daidaita nauyin rufin zinc da tsananin tsatsa. Muna ba da shawarar:
- Ƙasa mai ɗan lalata(pH 6-8, juriya >3000 ohm-cm): Rufin da aka yi amfani da shi wajen tsoma zafi na 460 g/m2
- Ƙasa mai tsatsa mai matsakaici(pH 5-6 ko juriya 1000-3000 ohm-cm): Rufin da aka yi zafi mai nauyi na 550 g/m2
- Ƙasa mai lalata sosai(pH <5 ko juriya <1000 ohm-cm): Yi la'akari da jan ƙarfe mai rufi ko bakin ƙarfe
Mataki na 4: Diamita da Tsawon.Muna ba da shawarar yin sanda mai kauri domin tana samar da babban wurin adana zinc, wanda ke tsawaita tsawon lokacin aiki. Diamita na yau da kullun yana tsakanin mm 14 zuwa 20, tare da tsayi daga mita 1.5 zuwa mita 3.0. A cikin ƙasa mai lalacewa sosai, hawa daga mm 14 zuwa mm 17.2 yana ƙara tsawon aiki mai ma'ana saboda kauri layin zinc yana ɗaukar lokaci mai tsawo kafin ya lalace.
Mataki na 5: Takardu.Kullum muna buƙatar takaddun shaida na injina waɗanda ke tabbatar da nauyin rufin, matakin ƙarfe, da kuma bin ƙa'idodin galvanizing na samfuranmu. Masana'antarmu tana ba da ISO 9001:2008 daAn ba da takardar shaidar ULtare da duk wani daftarin aiki da aka bayarsandunan ƙasa na ƙarfe mai galvanized, yana bawa abokan cinikinmu damar bin diddigin kayayyaki daga kayan da aka ƙera zuwa kayan da aka ƙera.
Ayyukan Shigarwa Waɗanda Ke Fadada Tsawon Rayuwar Sandar Ƙasa
Muna tunatar da abokan cinikinmu cewa ko da sandar ƙasa mafi kyau da aka ƙayyade ba za ta yi aiki ba idan shigarwar ta lalata murfin zinc ko kuma ta sanya sandar a cikin yanayi da ke hanzarta lalata. Kwarewarmu a fagen aiki a cikin nahiyoyi da yawa ta koya mana cewa ingancin shigarwa yana haifar da babban ɓangare na bambancin rayuwar sabis na sandar ƙasa.
Zurfin Tuki da Kariyar Sanda
Hanyar Tuki.Muna ba da shawarar amfani da murfin tuƙi ko kariya daga tip lokacin da muke buga sandar mu a ƙasa. Buga guduma kai tsaye zuwa ƙarshen sandar na iya ƙunsar murfin zinc kuma ya haifar da ƙarfe da aka fallasa a saman sandar. A cikin ƙasa mai duwatsu, muna ba da shawarar a haƙa rami kafin a fara haƙa sandar maimakon a tilasta mata ta hanyar toshewar da ke goge layin zinc. Muna haɗa tip ɗin tuƙi tare da jigilar sandar mu don taimakawa masu shigarwa su kare murfin yayin tuƙi.
Kayan Cika Baya.Ƙasa da ke kewaye da sandar tana da tasiri mafi girma kan yawan tsatsa. A cikin yanayin ƙasa mai tsauri, cika ramin sandar da kayan da ba su da juriya kamar yumbun bentonite ko siminti mai sarrafawa yana haifar da ambulaf mai kariya a kusa da sandar. Wannan cikawa yana rage hulɗar sandar da mafi munin sinadaran ƙasa na asali yayin da yake kula da haɗin wutar lantarki da ake buƙata don aikin ƙasa.IEEE 80 misaliyana ba da jagora kan tsarin tsarin ƙasa wanda ya haɗa da la'akari da abubuwan da suka shafi cike ƙasa.
Zurfi da Jagorori.Muna umurtar masu shigarwa da su tura sandar mu zuwa zurfin da ya dace domin saman sandar ya zauna aƙalla mm 150 ƙasa da matakin da aka gama. Sassan sandar da aka fallasa suna yin tsatsa da sauri a mahaɗin ƙasa da iska inda danshi da yawan iskar oxygen ke haifar da ƙwayar tsatsa daban-daban. Shigarwa a tsaye gabaɗaya yana yin tasiri ga kusurwoyin da aka tura domin yana sanya ƙarshen sandar a cikin yanayi mai zurfi da kwanciyar hankali na ƙasa.
Cikawa da Hanyoyin Haɗi
Kariyar Haɗi.Haɗin da ke tsakanin sandar ƙasa da mai sarrafa ƙasa yana nuna rauni idan aka bar shi a buɗe. Muna ba da shawarar a shafa tef ɗin hana lalata ko hannun riga mai rage zafi a kan mahaɗin injin don hana shigar da danshi. A masana'antarmu, muna samar da sanduna tare da igiyoyin kebul da aka haɗa waɗanda ke kawar da matsalar tsatsa ta haɗin gwiwa gaba ɗaya ta hanyar samar da wurin haɗin da aka yi da galvanized da aka yi da masana'anta.
Lokacin da za a Haɓaka: Madadin Rufin Tagulla ko Bakin Karfe
Mun yi imanin cewa sandunan ƙasa masu galvanized suna da amfani ga yawancin aikace-aikacen ƙasa. A cikin ƙasa mai matsakaicin ƙarfin tsatsa, sandar galvanized da aka ƙayyade da kyau tana ba da ingantaccen aiki a ƙaramin farashi na jan ƙarfe ko madadin bakin ƙarfe. Duk da haka, akwai ƙayyadaddun hanyoyin injiniya inda haɓakawa zuwa kayan da suka fi jure tsatsa yana haifar da sakamako mafi kyau na dogon lokaci.
Sandunan Rufi na Tagulla don Ƙasa Mai Tsanani
Sandunan da aka lulluɓe da tagullaYi amfani da layin jan ƙarfe mai haɗe da ƙwayoyin halitta a kan tsakiyar ƙarfe mai ƙarfi. Layin jan ƙarfe yana tsayayya da tsatsa a cikin yanayin acidic da mai yawan chloride inda rufin zinc ke ƙarewa da sauri. Sandar jan ƙarfe da aka lulluɓe yawanci tana ba da sabis na shekaru 30 zuwa 40 a cikin yanayin ƙasa wanda ke iyakance sandunan galvanized zuwa shekaru 8 zuwa 12. Layin jan ƙarfe kuma yana kiyaye ƙarancin juriyar ƙasa akan lokaci, wanda ke amfanar shigarwar lantarki mai mahimmanci.
Bakin Karfe don Muhalli Masu Tsanani
Sandunan bakin karfe(maki 304 da 316) suna samar da mafi girman juriya ga tsatsa tsakanin kayan sandar ƙasa. Karfe mai nauyin 316 na bakin ƙarfe yana jure yawan sinadarin chloride wanda ke lalata zinc da jan ƙarfe, wanda hakan ya sa ya zama zaɓi mafi kyau ga dandamalin teku, masana'antun sinadarai na bakin teku, da tsarin ruwa. Mun lura cewa farashin ciniki shine: sandunan bakin ƙarfe yawanci suna kashe sau 4 zuwa 8 fiye da na ƙarfen galvanized ɗinmu.
Muna ba abokan cinikinmu shawara da su yi amfani da tsarin yanke shawara mai sauƙi: ƙayyade sandunan galvanized lokacin da bayanan gwajin ƙasa ke tallafawa rayuwar sabis wanda ya dace da tsawon lokacin ƙirar kayayyakin more rayuwa. Lokacin da bayanan ƙasa suka nuna yanayi mai tsauri wanda zai buƙaci maye gurbin sandar a cikin jadawalin aikin, kwatancen farashi yana canzawa zuwa ga rufin jan ƙarfe ko bakin ƙarfe. Ƙungiyarmu tana ba da wannan bincike a matsayin wani ɓangare na tallafin injiniyan mu kafin siyarwa, kuma muna ba da duk zaɓuɓɓukan kayan aiki guda uku daga kewayon samfuranmu aXinchang Shibang.
An lulluɓe da ƙarfe mai kauri da ƙarfe mai kauri da ƙarfe mai kauri: Kwatanta Gefe-da-Gefe
Teburin da ke ƙasa ya taƙaita muhimman ayyuka da halayen farashi na manyan kayan sandar ƙasa guda uku. Muna ba da shawarar ku yi amfani da wannan a matsayin wurin farawa don zaɓar kayan, amma koyaushe muna ba da shawarar tabbatarwa da ainihin bayanan gwajin ƙasa daga wurin aikin ku.
| Kadara | An yi amfani da galvanized mai zafi | An lulluɓe da jan ƙarfe | Bakin Karfe |
|---|---|---|---|
| Babban Kayan Aiki | Q235 Carbon Karfe | Karfe Mai Ƙarfi | Bakin 304/316 |
| Rufi/Haɗaɗɗen abu | Zinc, microns 45-80 | Tagulla, microns sama da 250 | Gami mai ƙarfi |
| Rayuwar Sabis (Ƙaramin Ƙasa) | Shekaru 20-30 | Shekaru 30-40 | Shekaru 40+ |
| Rayuwar Sabis (Ƙasa Mai Lalacewa) | Shekaru 8-15 | Shekaru 25-35 | Shekaru 35-50 |
| Juriyar Chloride | Ƙasa zuwa Matsakaici | Mai kyau | Madalla sosai |
| Juriyar Ƙasa Mai Acid | Ƙasa | Mai kyau | Madalla sosai |
| Kudin Dangantaka | 1.0x (tushe) | 2.0-3.0x | 4.0-8.0x |
| Mafi kyawun Aikace-aikacen | Juyin ƙasa gabaɗaya a cikin ƙasa mai matsakaici | Kayayyakin more rayuwa na dindindin a cikin ƙasa mai tsauri | Muhalli na ruwa, sinadarai, da kuma yanayi mai tsauri |
Bayanin Masana'antar Shibang:Muna ƙera dukkan nau'ikan sanduna guda uku a cibiyarmu ta Xinchang.Q235 ƙarfe core galvanized ƙasa sandayana ba da ingantaccen aiki don aikace-aikacen ƙasa na yau da kullun. Ga abokan ciniki da ke fuskantar tsatsa mai tsanani a ƙasa, muna samar da sandunan ƙarfe masu lulluɓe da na jan ƙarfe tare da kewayon galvanized ɗinmu. Tuntuɓi ƙungiyar injiniyanmu tare da bayanan gwajin ƙasa, kuma za mu ba da shawarar samfurin da ya fi dacewa da yanayin wurinku.
Tambayoyin da Ake Yawan Yi Game da Lalata Sanda Mai Gina Ƙasa
Tsawon wane lokaci sandar ƙasa mai galvanized za ta daɗe a cikin ƙasa mai lalata?
Tsawon rayuwar sandar ƙasa mai galvanized a cikin ƙasa mai lalata ya dogara sosai akan nauyin murfin zinc, sinadaran ƙasa, da matakan danshi. Sandar lantarki mai siririn zinc na yau da kullun na iya nuna tsatsa a bayyane cikin shekaru 2 zuwa 5 a cikin yanayin ƙasa mai tsauri kamar yankunan bakin teku masu arzikin chloride ko laterite na wurare masu zafi masu acidic. Sandar galvanized mai zafi mai nauyin rufi na 550 g/m2 ko sama da haka yawanci tana ba da shekaru 15 zuwa 25 na aiki a cikin yanayi mai laushi. A cikin ƙasa mai tsananin ƙarfi, har ma sandunan galvanized masu zafi na iya buƙatar maye gurbinsu cikin shekaru 10 zuwa 12. Ƙungiyar injiniyanmu a Shibang ta ba da shawarar gudanar da binciken juriyar ƙasa da pH kafin zaɓar kowane samfurin sandar ƙasa. Muna ƙera sandunan ƙasa masu galvanized masu zafi tare da kauri zinc mai daidaito don ba wa abokan cinikinmu tsawon rai na sabis a fagen.
Mene ne bambanci tsakanin sandunan ƙasa masu amfani da lantarki da kuma waɗanda aka yi amfani da su a cikin ruwan zafi?
Na'urar lantarki mai amfani da wutar lantarki tana sanya siririn zinc a saman ƙarfe ta hanyar amfani da hanyar lantarki, wanda yawanci ke samar da kauri daga microns 5 zuwa 15. Na'urar lantarki mai amfani da wutar lantarki tana nutsar da sandar ƙarfe a cikin zinc mai narkewa a kimanin digiri 450 na Celsius, tana samar da shafi na microns 45 zuwa 80 ko fiye dangane da lokacin nutsewa da sigogin aiki. Rufin da ke da kauri na nutsewa yana ƙirƙirar haɗin ƙarfe tsakanin zinc da ƙarfe, wanda ke tsayayya da barewa kuma yana ba da kariya ta sadaukarwa na tsawon lokaci. A masana'antarmu, muna amfani da na'urar lantarki mai amfani da wutar lantarki ga sandunanmu na ƙasa; layin zinc mai kauri, wanda aka haɗa yana aiki mafi kyau a cikin ƙasa mai lalata. Sandunan lantarki suna kama da juna a saman amma suna yin lalata da sauri a ƙarƙashin ƙasa, wanda ke haifar da gazawar sandar ƙasa da wuri.
Ta yaya zan gwada lalata ƙasa kafin in zaɓi sandar ƙasa?
Gwajin gurɓataccen ƙasa ya ƙunshi auna pH, juriya, yawan danshi, yawan sinadarin chloride, da matakan sulfate a zurfin shigarwa da aka tsara. Gwajin juriyar ƙasa mai lamba huɗu na Wenner yana ba da karatun juriyar tushe, yayin da nazarin gwaje-gwaje na samfuran ƙasa ke nuna abubuwan da ke cikin sinadarai. Ma'aunin ANSI/NACE SP0169 da jagorar IEEE 80 duk sun bayyana hanyoyin rarraba ƙarfin ƙasa. Ƙasa mai juriya a ƙasa da santimita 1000 ohm, pH a ƙasa da 5.5, ko babban abun ciki na chloride suna cikin mawuyacin hali. Muna ba abokan cinikinmu shawara su gudanar da waɗannan gwaje-gwajen a zurfafa da yawa, yayin da sinadaran ƙasa ke canzawa yayin da kuke zurfafawa. Ƙungiyar tallace-tallace tamu a Shibang tana amfani da bayanan ƙasa daga wurin abokin ciniki don ba da shawarar madaidaicin nauyin rufi da kayan sanda, don tabbatar da cewa sandar ƙasa mai galvanized ta dace da ainihin yanayin filin maimakon dogaro da ƙayyadaddun bayanai na gabaɗaya.
Za a iya amfani da sandunan ƙasa na galvanized a yankunan bakin teku?
Sandunan ƙasa masu galvanized suna aiki a yanayin bakin teku, amma tsawon lokacin aikinsu yana raguwa sosai idan aka kwatanta da shigarwar cikin gida. Ƙasa da ruwan ƙasa suna ɗauke da yawan ions na chloride, waɗanda ke kai hari ga murfin zinc da hanzarta lalata sandar ƙasa mai galvanized. A cikin ƙwarewarmu ta samar da ayyuka a Gabas ta Tsakiya da Kudu maso Gabashin Asiya, mun ga sandunan lantarki masu sirara masu lulluɓe da electro-galvanized sun faɗi cikin shekaru 3 a cikin ƙasa mai yawan chloride. Sandunan galvanized masu lulluɓe da zafi tare da murfin zinc masu nauyi suna aiki mafi kyau amma har yanzu suna buƙatar sa ido da maye gurbinsu daga ƙarshe. Don kayayyakin more rayuwa na dindindin na bakin teku kamar tashoshin ƙasa da kuma shimfida dandamali na ƙasashen waje, ƙungiyar injiniyanmu sau da yawa tana ba da shawarar haɓakawa zuwa madadin jan ƙarfe ko bakin ƙarfe. Duk da haka, don shigarwa na ɗan lokaci ko ayyuka tare da ƙayyadaddun lokutan sabis, sandar ƙasa mai galvanized mai lulluɓe da zafi tare da matsakaicin kauri zinc tana ba da mafita mai amfani da tattalin arziki.
Wane nauyin rufin zinc ya kamata in ƙayyade don ƙasa mai tsauri?
Don yanayin ƙasa mai tsauri, muna ba da shawarar a sami mafi ƙarancin nauyin murfin galvanized mai zafi na gram 550 a kowace murabba'in mita (g/m2), wanda ya yi daidai da kimanin microns 80 na kauri na zinc. Wannan ƙayyadaddun ya yi daidai da buƙatun da aka tsara a cikin ma'auni kamar ISO 1461 da ASTM A123. A cikin yanayi mai tsanani kamar ƙasa mai yawan chloride a bakin teku ko kuma tarkacen peat mai acidic, ƙayyade 610 g/m2 ko sama da haka yana ba da ƙarin gefe. Sandar ƙasa mai ƙarfi ta ƙarfe ta Q235 a Shibang tana amfani da tsarin tsoma zafi mai sarrafawa don cimma daidaiton nauyin shafa a kowane rukunin samarwa. Muna gwada kauri na shafa a kowane yanki ta amfani da hanyoyin auna maganadisu kuma muna ba da takaddun shaida na niƙa tare da kowane jigilar kaya. Bayyana madaidaicin nauyin shafa a matakin siye yana hana mafi girman farashin maye gurbin sandunan da suka gaza bayan shigarwa.
Ta yaya pH na ƙasa ke shafar tsawon rayuwar sandar ƙasa mai galvanized?
pH na ƙasa yana tasiri kai tsaye kan yadda murfin zinc akan sandar ƙasa ke narkewa. A cikin ƙasa mai ƙarfi mai acidic (pH ƙasa da 4.5), ions na hydrogen suna amsawa da ƙarfi tare da layin zinc, suna narkar da shi da sauri kuma suna fallasa tsakiyar ƙarfe ga tsatsa. A cikin ƙasa mai alkaline (pH sama da 8.5), zinc yana samar da Layer oxide mai aiki wanda ke rage tsatsa, amma yawan carbonate ko sulfate a cikin ƙasa mai alkaline har yanzu yana iya haifar da ramuka na gida. Rufin zinc yana aiki mafi kyau a cikin ƙasa mai kusan tsaka tsaki (pH 6 zuwa 8) inda ƙimar narkewar ta kasance ƙasa kuma patina mai kariya ta kasance ba tare da matsala ba. Masana'antarmu tana sarrafa tsarin galvanizing don samar da Layer ɗin ƙarfe mai kama da zinc wanda ke tsayayya da harin acidic fiye da rufin zinc mai tsabta. Muna ba abokan ciniki shawara su haɗa bayanan pH na ƙasa tare da juriya da ma'aunin chloride don cikakken hoto na yanayin tsatsa kafin yin oda.
Yaushe ya kamata in canza daga sandunan ƙasa masu galvanized zuwa sandunan ƙasa masu lulluɓe da tagulla?
Shawarar canzawa daga sandunan ƙasa da aka lulluɓe da jan ƙarfe zuwa sandunan ƙasa da aka lulluɓe da jan ƙarfe ya dogara da tsawon lokacin sabis ɗin da ake buƙata, tsananin tsatsa na ƙasa, da kuma kasafin kuɗin aikin. Idan gwajin ƙasa ya nuna juriya a ƙasa da santimita 500 na ohm tare da matakan chloride ko sulfate masu yawa, sandunan galvanized ba za su iya samar da tsawon shekaru 25 na sabis kamar yadda takamaiman bayanai da yawa ke buƙata ba. Sandan jan ƙarfe da aka lulluɓe da jan ƙarfe suna amfani da layin jan ƙarfe da aka lulluɓe da ƙwayoyin halitta a kan tsakiyar ƙarfe, suna ba da kyakkyawan juriya ga tsatsa a cikin ƙasa mai ƙarfi yayin da suke riƙe da ƙarfin injin ƙarfe. A cikin ƙwarewarmu ta tallafawa ayyuka a Kudu maso Gabas na Asiya da Gabas ta Tsakiya ta bakin teku, sandunan jan ƙarfe da aka lulluɓe suna ɗaukar shekaru 30 zuwa 40 a cikin yanayi inda sandunan galvanized suka gaza cikin shekaru 8 zuwa 12. Muna ba da shawarar sandunan jan ƙarfe da aka lulluɓe don kayayyakin more rayuwa na dindindin kamar tashoshin wutar lantarki, cibiyoyin bayanai, da hasumiyoyin sadarwa inda maye gurbin sandunan ƙasa bayan aiki zai zama mai rikitarwa da tsada.
Me ke haifar da gazawar sandar ƙasa da wuri a filin wasa?
Rashin nasarar sandar ƙasa da wuri yawanci yana faruwa ne sakamakon rashin daidaito tsakanin ƙayyadaddun sandar da ainihin yanayin ƙasa a wurin shigarwa. Manyan abubuwan da muke fuskanta sun haɗa da ƙarancin kauri na zinc don sinadaran ƙasa, amfani da sandunan lantarki masu galvanized inda ake buƙatar samfuran tsoma zafi, shigarwa mara kyau wanda ke lalata murfin zinc yayin tuki, da kuma rashin la'akari da canjin danshi na yanayi wanda ke tattara sinadarai masu lalata kusa da saman sandar. Lalacewar injiniya yayin shigarwa, kamar buga sandar ta cikin ƙasa mai duwatsu ba tare da tip ɗin tuƙi ba, na iya cire murfin zinc a wurin da aka taɓa, yana ƙirƙirar ƙwayar tsatsa ta gida. A yankunan arewacin Turai na permafrost, zagayowar daskarewa-narkewa yana haifar da motsi na ƙasa wanda ke ƙarfafa sandar kuma yana iya fasa layin zinc. Ƙungiyarmu ta fasaha a Shibang tana ba da jagorar shigarwa tare da kowane oda don taimakawa abokan cinikinmu su guji waɗannan hanyoyin gazawar da za a iya hanawa.
Jane Yang
Manajan Talla a Xinchang Shibang New Material Co., Ltd.
Wannan Jane ce daga Xinchang Shibang New Material Co., Ltd wacce ƙwararriyar masana'anta ce ta samar da kayayyakin ƙasa da tsarin walƙiya sama da shekaru 17.
Ni manajan tallace-tallace ne mai shekaru 12 na gwaninta a fannin kare walƙiya da kuma dakatar da cinikin ƙasashen waje.
Na ƙware wajen tallafawa abokan ciniki na ƙasashen waje ta hanyar samo kariyar walƙiya da kayayyakin ƙasa daga China, waɗanda suka shafi cikakkun ayyuka, gami da duba inganci, shirya kayayyaki da duk takardun fitarwa. Haka kuma zan iya taimaka muku wajen siyan wasu kayayyaki masu alaƙa da wutar lantarki.
ƙwararre, abin dogaro kuma mai sauƙin mu'amala da shi, ina shirye in ba ku mafita ta siye ɗaya.